S275JR CHEMICAL COMPOSITION (%) | ||||||||
C | Mn | P | S | Si | Cr | Ni | Mo | N |
≤0.37 | ≤1.5 | ≤0.035 | ≤0.05 | ≤0.15 | ≤0.3 | ≤0.30 | / | ≤0.014 |
S275JR MECHANICAL PROPERTIES | |||||
Yield Strength | Tensile Strength | Elongation | Hardness | ||
HB | HRB | HV | |||
≧275 | 430-580 | ≧12 | ≤187 | ≤90 | ≤200 |